Like we just got the feed pellet mill, it is recommended that the first break-in operation, with oil to granulate, the operation of half an hour an hour, according to the situation of the material, the material is normal in the normal production.
Otherwise, it is likely that the late production is too low, easy to clog. Like granules have cracks because the raw material moisture content is too high. If there is a lot of dust, it is the opposite, because the water content of raw materials is too low. You need to have a measure of the water content of the raw material in your mind. Like the feed pellet machine has a noise or sudden stop, it is likely to be into the hard stuff caused by the noise or stop, but also may be a short circuit caused by the stop.